Zhejiang Weilan Technology Co., Ltd.

Sodium Hypochlorite Dosing: PVDF vs PVC Pump Heads & Auto-Degassing Valves

Author: Zhejiang Weilan Technology Co., Ltd.Source: Official sitePublished: Category: News
Summary: Why PVDF auto-degassing pump heads outlast PVC in bleach disinfection systems by preventing UV embrittlement, micro-cracking, and oxygen gas lock.

Sodium hypochlorite (NaClO, 5%–12%) continuously decomposes into oxygen micro-bubbles while attacking plastics oxidatively. Standard PVC pump heads often turn brittle and crack around tie-bolts within 6–18 months in warm or sunlit installations.

1. PVC vs PVDF Head Lifespan

  • PVC: Lower upfront cost, acceptable for indoor, cool, short-term use, but prone to oxidative stress cracking above 40 °C or under UV exposure.
  • PVDF: Superior resistance to strong oxidizers, UV light, and temperatures up to 60–80 °C, typically lasting 3–5× longer than PVC in continuous bleach service. Pair with PTFE diaphragms, FKM seals, and ceramic or PTFE check balls (never SS316L).

2. Auto-Degassing Heads Stop Air-Lock

Oxygen bubbles accumulate at the top of the pump chamber during idle periods, causing air-lock on restart. An auto-degassing solenoid head continuously vents trapped gas back to the tank via a small return tube.

Conclusion

Specify PVDF auto-degassing heads, FKM seals, and softened dilution water to eliminate bleach scaling and air-lock. Explore Products or Contact Us.

FAQ

Can I use stainless steel 316L check balls for sodium hypochlorite?

No. Active chloride ions pit SS316L rapidly; always specify alumina ceramic, glass, or PTFE check balls.

Why does my injection quill clog with white scale?

Hard dilution water precipitates calcium carbonate in alkaline bleach; dilute with RO/softened water and descale the injection check valve every 1–2 months.

Get a Quote

Leave your requirements and we will reply within 1 business day