RO Dechlorination Dosing Pump Selection and ORP Interlock Guide
Polyamide reverse osmosis (RO) membranes suffer irreversible oxidation damage if exposed to free chlorine above 0.1 mg/L. Installing a reliable RO dechlorination pump dosing sodium metabisulfite (SMBS) ahead of the high-pressure pump protects membrane salt rejection.
Here is how to size the pump, tune inline ORP control, and avoid bacterial biofouling from overdosing.
1. SMBS Dosing Sizing and PVDF Wetted Parts
Stoichiometrically, 1.47 mg/L of pure SMBS neutralizes 1 mg/L of free chlorine; plants typically dose 3 to 4 times the residual chlorine concentration for complete reaction before the cartridge filter. For 5–50 m³/h RO feeds, dilute batches 10–20x and use a 1–10 L/h (5–10 bar) PVDF-head solenoid pump (SEKO Tekna APG or New Dose EvoDose) with PTFE diaphragm and FKM seals.
2. Closed-Loop ORP Setpoints and Feed-Pump Interlock
Complete dechlorination drops water ORP into the 150–250 mV band. Drive the RO dechlorination pump via 4-20mA from an inline ORP transmitter so dosing rises above 280 mV and cuts back below 150 mV—preventing excess SMBS from stripping dissolved oxygen and feeding anaerobic membrane biofouling. Hard-wire power to the main RO feed booster pump contactor.
3. Lidded Tanks and 3–7 Day Fresh Batches
Exposure to air oxidizes SMBS into inactive sulfate. Mix 3–7 day batches using RO permeate in tightly lidded opaque PE tanks, and rinse check valves monthly.
Conclusion
Combining PVDF metering pumps, 150–250 mV ORP proportional control, and fresh lidded batches ensures reliable RO dechlorination pump protection. Visit Products or Contact Us for packaged RO dechlorination skids.
FAQ
Should SMBS be injected before or after RO antiscalant?
Inject at separate points upstream of the cartridge filter (typically dechlorination first, antiscalant second) so concentrated chemicals never mix directly in one tee.
Why did RO differential pressure climb faster after starting SMBS?
Chronic overdosing (ORP < 100 mV) scavenges oxygen and fuels anaerobic slime on cartridge filters and membranes; verify ORP calibration and trim dosing factor.
Is a faint sulfur dioxide odor near the SMBS tank normal?
Yes. Keep tank lids sealed tightly and vent the dosing room to protect nearby electronics from acidic vapor.
How do I clear yellow crystals inside SMBS suction tubing?
Flush with warm clean water for 5 minutes and keep diluted solution strength below 10%–15%.
Do you supply complete RO dechlorination skids with ORP controllers?
Yes, we supply 7–10 bar PVDF metering pumps, industrial ORP controllers, and 60–200 L lidded tanks.