Heavy Metal Chelating Agent (DTCR) Dosing Pump: Materials and Control
When hydroxide precipitation alone cannot push electroplating nickel, copper, or lead below strict discharge limits (< 0.1 mg/L), plants dose organic sulfur heavy metal chelating agent (DTCR or TMT-15). Because the reagent is costly, alkaline, and reacts instantly with trace metals, choosing the right pump materials prevents internal fouling.
Here is how to specify and pipe a DTCR metering pump properly.
1. Zero Brass or Iron Contact: Use Plastic + EPDM
- Avoid all copper, brass, and carbon steel fittings:
DTCRchelates metal ions directly on contact; any brass union or iron valve will corrode while precipitating sticky black metal-sulfide sludge inside the check valves. - Specify
PVCorPVDFheads withEPDMseals: BecauseDTCRsolutions sit atpH 10–13, pairPVDForPVCheads and ceramic balls with alkali-resistant EPDM O-rings.
2. Neat vs Diluted Dosing Pump Selection
For neat viscous concentrate, choose a low-RPM mechanical diaphragm pump (KEMPION KS/AX1 or SEKO Spring MS1) with flooded suction and upsized tubing. When diluted 10–20x to a 5%–10% solution for better tank dispersion, standard 2–20 L/h PVDF solenoid pumps (Tekna APG or EvoDose) work reliably.
3. Flow-Proportional Pacing to Control Chemical Cost
Pace pump speed via 4-20mA from the influent flowmeter and run weekly jar tests to avoid over-dosing, which wastes expensive reagent and slightly elevates effluent COD.
Conclusion
Eliminating metal fittings, specifying PVC/PVDF with EPDM seals, and pacing flow proportionally keep heavy metal chelating agent dosing economical and clog-free. Visit Products or Contact Us for alkali-rated dosing skids.
FAQ
Is a faint sulfurous odor around the DTCR day tank normal?
Yes, organic sulfur chelators carry a mild odor; keep day tanks lidded and ventilated.
How should black sludge buildup inside check valves be cleaned?
Flush thoroughly with warm water first; never pour strong acid directly onto concentrated DTCR, as acidifying neat DTCR releases toxic hydrogen sulfide (H2S) gas.
Should DTCR be dosed before or after PAC coagulant?
Dose DTCR after pH adjustment, allow 10–15 minutes mixing for complete chelation, and then add PAC and PAM to settle the micro-flocs.
Can SS316L stainless pump heads handle DTCR?
PVC or PVDF plastic heads are preferred because they cost less and eliminate all risk of trace metal leaching.
Do you supply complete DTCR dilution tanks with EPDM-sealed pumps?
Yes, we supply 100–500 L lidded mixing tanks paired with EPDM-sealed PVDF metering pumps.